Due to high chromium steel, and its anti-oxidation and corrosion resistance is superior to low-alloy steel, but the strong performance of hot steel 2.25Cr-1Mo steel below. Poor weldability.
Applications:
High-temperature sulfur corrosion, high temperature naphthenic acid corrosion.
Wall temperature of ≤ 630 ℃ reheater tube.
Standards: ASTM A213/ASTM A335
Material specifications of origin
Cr9Mo/P9/T9 76-114x4-30 A335 Baosteel / import
Cr9Mo/P9/T9 133-168x4-30 A335 Baosteel / import
Cr9Mo/P9/T9 219-820x10-70 A335 Chengdu / import |
|