Are heat-resistant stainless steel Grade Comparison China Brand: 0Cr18Ni10Ti Japan Brand: SUS321 U.S. Brand: 321 Germany Brand: 1.4541 Chemical composition: C <= 0.08, Mn <= 2.00, Si <= 1.00, P <= 0.045, S <= 0.030, Ni9.00 ~ 13.00, Cr17.00 ~ 19.00, Ti> = 5xC% Solid solution heat treatment, the yield strength> = 205, tensile strength> = 520 (hardness HB <= 187), elongation> = 40. Scope of application: Intergranular corrosion resistance is better, so 400 ~ 900 degrees of corrosion of the components under the conditions of use, high-temperature welding structure
Cold :0.5-3 * 1219 * C
Hot-rolled :3-60 * 1500 * 6000 |
|